Near-miss: Welding in ‘no hot work’ zone
A member has reported a near miss incident in which welding was discovered which had clearly taken place in a ‘no hot work’ zone. The welding was discovered during pre-sail departure checks of the main deck. The Chief Officer noticed dogging plate welds securing a half-height container had been welded on to a ‘no hot work’ zone on the deck.
Our members’ initial finding was that the task was not properly planned or supervised, allowing sea-fastenings to be welded on to a ‘no hot-work’ zone.
Members may wish to refer to the following incident (search word: hot work zone):
Safety Event
Published: 20 September 2016
Download: IMCA SF 24/16
IMCA Safety Flashes
Submit a Report
IMCA Safety Flashes summarise key safety matters and incidents, allowing lessons to be more easily learnt for the benefit of all. The effectiveness of the IMCA Safety Flash system depends on Members sharing information and so avoiding repeat incidents. Please consider adding safetyreports@imca-int.com to your internal distribution list for safety alerts or manually submitting information on incidents you consider may be relevant. All information is anonymised or sanitised, as appropriate.
IMCA’s store terms and conditions (https://www.imca-int.com/legal-notices/terms/) apply to all downloads from IMCA’s website, including this document.
IMCA makes every effort to ensure the accuracy and reliability of the data contained in the documents it publishes, but IMCA shall not be liable for any guidance and/or recommendation and/or statement herein contained. The information contained in this document does not fulfil or replace any individual’s or Member's legal, regulatory or other duties or obligations in respect of their operations. Individuals and Members remain solely responsible for the safe, lawful and proper conduct of their operations.